HARDNESS COMPARISON
(Based on ASTM A623)
Designation
T-1
T-2
T-3
T-4
T-5
DR-8
DR-9
Aim Rockwell Range (30-T Scale)
46-52
50-56
54-60
58-64
62-68
73
76
TEMPER CLASSIFICATION
DR480
=
DR7
DR520
=
DR7 / DR8
DR550
=
DR8
DR580
=
DR8M / DR9
DR620
=
DR9
DR660
=
DR9M
DR690
=
DR10
TS245
=
T2.5
TH245
=
T57 OR T3
TS 260
=
T55 OR T3
TS275
=
T57 OR T3
TH370
=
T61 OR T4
TH415
=
T61 OR T4
TH435
=
T65 OR T5
TS480
=
T65 OR T5
TH520
=
DR520CA
TH550
=
DR550CA
TS550
=
DR550BA
TH580
=
DR580CA
TH620
=
DR620CA
TIN COATING WEIGHTS
(Based on ASTM A624)
Designation
lbs/BB
g/m
2
Designation
lbs/BB
g/m
2
10
0.05/0.05
1.1/1.1
50/25
0.25/0.125
5.6/2.8
20
0.10/0.10
2.2/2.2
75/25
0.375/0.125
8.4/2.8
25
0.125/0.125
2.8/2.8
75/50
0.375/0.25
8.4/5.6
35
0.175/0.175
3.9/3.9
100/25
0.50/0.125
11.2/2.8
50
0.25/0.25
5.6/5.6
100/50
0.50/0.25
11.2/5.6
75
0.375/0.375
8.4/8.4
100/75
0.50/0.375
11.2/8.4
100
0.50/0.50
11.2/11.2
135/25
0.675/0.125
15.2/2.8
FINISH
(Based on ASTM STANDARDS)
7B
BRIGHT
7C
STONE
5C
SILVER
5C /5D
MATTE
DECIMAL EQUIVALENTS
Fraction
Decimal
Millimeter
1/16
0.0625
1.5875
1/8
0.1250
3.1750
3/16
0.1875
4.7625
1/4
0.2500
6.3500
5/16
0.3125
7.9375
3/8
0.3750
9.5250
7/16
0.4375
11.1125
1/2
0.5000
12.7000
9/16
0.5625
14.2875
5/8
0.6250
15.8750
11/16
0.6875
17.4625
3/4
0.7500
19.0500
13/16
0.8125
20.6375
7/8
0.8750
22.2250
15/16
0.9375
23.8125
1
1.0000
25.4000